牌号简介 About |
---|
LNP™ THERMOTUF™ PX06417是一种基于尼龙6树脂的化合物,含有40%的玻璃纤维。这种材料的附加特性包括:热稳定、高冲击、紫外线稳定。又名:LNP™ THERMOTUF™化合物PF-1008 hi-hs紫外线产品再订购名称:PX06417 LNP THERMOTUF PX06417 is a compound based on Nylon 6 resin containing 40% Glass Fiber. Added features of this material include: Heat Stabilized, High Impact, UV Stabilized. |
产品描述 Product Description
厂家:沙特沙伯基础 SABIC
类别:PA6 PA6
加工条件:注射成型 Injection Molding
性能特点: 防火阻燃等级HB; 热稳定性好; 冲击性能好; 耐候抗UV; Weather resistance is good,High impact resistance,Heat Stabilized,HB
紫外线:UV Stabilized
填料:玻璃纤维 40
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
1.46 | g/cm³ | ASTM D792 |
密度 Density |
1.46 | g/cm³ | ISO 1183 |
收缩率 Shrinkage rate |
ISO 294-4 | ||
TD:24 hrs TD:24 hrs |
0.90 | % | ASTM D955 |
MD:24 hrs MD:24 hrs |
0.20 | % | ASTM D955 |
TD:24 hrs TD:24 hrs |
0.93 | % | ISO 294-4 |
MD:24 hrs MD:24 hrs |
% | ISO 294-4 | |
吸水率 Water absorption rate |
|||
平衡,23℃,50% RH Equilibrium, 23 ℃, 50% RH |
% | ISO 62 | |
24hr,50% RH 24hr,50% RH |
% | ASTM D570 | |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸模量 Tensile modulus 2 |
MPa | ASTM D638 | |
拉伸模量 Tensile modulus |
MPa | ISO 527-1-2 | |
拉伸强度 tensile strength |
|||
断裂 fracture |
MPa | ASTM D638 | |
断裂 fracture |
MPa | ISO 527-2 | |
拉伸应变 Tensile strain |
|||
断裂 fracture |
% | ASTM D638 | |
断裂 fracture |
% | ISO 527-2 | |
弯曲模量 Bending modulus |
MPa | ASTM D790 | |
弯曲模量 Bending modulus |
MPa | ISO 178 | |
弯曲强度 bending strength |
MPa | ASTM D790 | |
弯曲强度 bending strength |
MPa | ISO 178 | |
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
悬臂梁缺口冲击强度 Impact strength of cantilever beam notch |
|||
23℃ 23℃ |
J/m | ASTM D256 | |
23℃ 23℃ 3 |
kJ/m² | ISO 180-1A | |
23℃ 23℃ |
J/m | ASTM D4812 | |
悬臂梁无缺口冲击强度 Notched impact strength of cantilever beam 3 |
|||
23℃ 23℃ 3 |
kJ/m² | ISO 180/1U | |
装有测量仪表的落镖冲击 Dart impact equipped with measuring instruments |
|||
23℃,Energy at Peak Load 23℃,Energy at Peak Load |
J | ASTM D3763 | |
多轴向仪器化冲击能量 Multi axial instrumented impact energy |
J | ISO 6603-2 | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热变形温度 Hot deformation temperature |
|||
1.8 MPa,未退火,64 mm跨距 1.8 MPa, unannealed, 64 mm span 4 |
℃ | ISO 75-2/Af | |
1.8 MPa,未退火,3.2 mm 1.8 MPa, unannealed, 3.2 mm |
℃ | ASTM D648 | |
0.45 MPa,未退火,3.2 mm 0.45 MPa, unannealed, 3.2 mm |
℃ | ASTM D648 | |
线性热膨胀系数 Linear coefficient of thermal expansion |
|||
TD:-40~40℃ TD:-40~40℃ |
1/℃ | ASTM E831 | |
TD:-40~40℃ TD:-40~40℃ |
1/℃ | ISO 11359-2 | |
MD:-40~40℃ MD:-40~40℃ |
1/℃ | ASTM E831 | |
MD:-40~40℃ MD:-40~40℃ |
1/℃ | ISO 11359-2 | |
阻燃性能 FLAME CHARACTERISTICS |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
阻燃等级 Flame retardant level |
|||
1.50 mm 1.50 mm |
UL 94 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 2.0 in/min |
3 80*10*4 |
4 80*10*4 mm |
【新闻资讯】查看全部
美迷信家称塑料瓶含内分泌搅扰物质影响发育
2016-10-24 据外媒报道,上周二美国科学家发布报告指出,塑料瓶中的内分泌干扰物质可能导致癌症、糖尿病、注意力不足多动症(ADHD)以及自闭症,每年还让美国损失3400亿美元。 美科学家称塑料瓶含内 |
美迷信家称塑料瓶含内分泌搅扰物质影响发育 据外媒报道,上周二美国生物学家公布汇报强调,塑料瓶子中的内分泌干扰物质很有可能导致癌病、糖尿病患者、专注力不够儿童多动症(ADHD)及其儿童自闭症,每一年还让美国损害3400亿美金。 美生物学家称塑料瓶子含内分泌干扰物质危害生长发育 据报道,内分泌干扰物质会干扰人体激素系统软件,危害生长发育,易让人体患多种多样病症;美国美国的大学朗格尼研究中心(Langone Medical Center)的研究发现,从塑胶与金属材料食品包装材料,到清洁液、小玩具、护肤品上都带有这类有害物质。 内分泌干扰物质最常损害中枢神经系统,会导致专注力不够过动症(ADHD)与儿童自闭症、智商缺失等,也会提升糖尿病患者、过胖、男性不育、孑宫内膜异位症与一部分癌病风险性。 此次科学研究还表明了内分泌干扰物质对经济发展的危害。汇报称,这种物质导致的身心健康病症每一年让美国损害3400亿美金。 来源于:我国塑料机械网 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |
价格走势图
开始时间:
结束时间:
材料厂家:
【牌号齐全,内容全面】
全网共2500+项牌号+上游原料单体+原油价格,最长可追溯近20年价格行情
【精准,及时,权威!】
专业团队挖掘行情信息,第一时间发布行情
抱歉!该牌号暂无认证数据。
免责声明:参考价格是搜料网根据网络大数据拟合分析的结果,仅供参考。实际成交价取决但不限于以下因素:下单时间,付款方式,交货方式,数量,税费,色号,产地,项目信息。
抱歉!暂无数据。
抱歉!暂无数据。